T 815- TECHNO BASE EPOXY ZINK PHOSPHATE

T656   - TECHNO SANDING SEALER

One component nitrocellulose sanding clear primer, special for wood

DESCRIPTION               : An excellent quality two-component epoxy primer based on Polyamide  cured Epoxy resin.It has the following features ,excellent        adhesion with steel surfaces, excellent anti-corrosive property. Salt, Alkali and acid solu- tion resistance propertiesan very good solvent resistance property.
 RECOMMENDED USE      : Recommended   to   use     on   steel   surface     for   exterior   and     interior applications as an anti-corrosive primer.
  TECHNICAL INFO
Density 1.5 (mixed paint) at temperature 25°C , ASTM D-1475.
Viscosity 95-96 KU (Mixed Paint) at temperature 25°C, ASTM D-562.
Solid content 60 %(by volume) . ASTM D-5201.
Spreading Rate Theoretical spreading rate: 12 m²/L at D.F.T. 50 µ.
Hardness Pass, 4 H Pencil, ASTM D-3363.
Scratch Resistance Pass, 1 Kg., ASTM D-5178
Bending Pass 3 mm. Diameter, ASTM D-522.
Adhesion Pass, ASTM D-3359, and 400 psi, ASTM D-4541-III.
Impact Pass, 1 kg. / 1 meter / 16.3 mm. Diameter, ASTM D-2794.
Water Resistance Pass, ASTM D-870.
Chemical Resistance Pass, ASTM D-1308.
Mixing ratio By volume: Base to Hardener, 3: 1.
POTLIFE 6 Hours at 25°C. (after mixing).
INDUCTION TIME 20-30 minutes @ 25 °C.
DRYING TIME Dry to touch: 2 hours.
Recoating Interval Minimum 12 hours
Maximum 30 Days.
Full cure 7 Days.All above drying time tested according to ASTM D-5895.
THINNER Recommended Thinner is “Techno Thinner T899”.
   

APPLICATION GUIDE




APPLICATION TOOLS THINNING RATIO



PACKING

SHELF LIFE

Prepare the surface properly.
Mix the base paint and hardener according to mixing ratio uniformly.
Thin the mixed paint according to thinning ratio as per specification.
Apply one coat of “Techno Epoxy Phosphate” on steel surfaces.
Air Spray:- Thinning Ratio: (20 – 30) % by volume. Nozzle Size: (1.5 – 1.8) mm.
Nozzle Size: (1.5 – 1.8) mm.
Airless Spray:- Thinning Ratio: (0 – 10) % By volume for (75 – 100) μ
D.F.T. (10 – 20)% By volume for (50 – 70) μ D.F.T.
Nozzle Size: 0.48 mm. (approximately).
Roller / Brush:- Thinning Ratio: (15 – 20) % by volume.
Gallons: Base 2.70 Ltr, Hardener 0.90 Ltr.


18 Ltr. Drum: Base 13.50Ltr, Hardener 4.50Ltr.

In sealed container: 12 months in dry, cool, and well ventilated place.

 
 